Testing of low temperature behaviour of asphalt mixtures in bending creep test

The paper presents a method of bending beam test and its importance for evaluation of asphalt mixtures behaviour at low temperatures. Two types of asphalt mixtures: asphalt concrete AC with normal paving grade bitumen and stone mastic asphalt SMA with SBS-modified bitumen were tested. Long-term oven ageing (LTOA) test was also used in the laboratory according to SHRP procedure. The Burgers model was applied and rheological parameters of asphalt mixtures were determined in range of temperature from -10ºC to 10ºC. It has been found that the theoretical Burgers model fits well the experimental data obtained from the creep test. The testing method of bending beam under constant load was relatively simple and easy to use. The paper presents the method of testing, numerical results and analysis of data.

Authors

Additional information

DOI
Digital Object Identifier link open in new tab 10.1201/9780203092989.ch30
Category
Aktywność konferencyjna
Type
materiały konferencyjne indeksowane w Web of Science
Language
angielski
Publication year
2009

Source: MOSTWiedzy.pl - publication "Testing of low temperature behaviour of asphalt mixtures in bending creep test" link open in new tab

Portal MOST Wiedzy link open in new tab