This paper investigates the methodology for differentiation of multistep process of pitting corrosion of AISI 304 stainless steel in the environment of iron (III) chloride. Measurements were performed using Galvanodynamic Electrochemical Impedance Spectroscopy (GDEIS). Application of this methodology allowed monitoring of natural corrosion process without external current (IDC = 0A) nor potential perturbation of the system. Applied sinusoidal AC current does not influence significantly registered DC potential. Analysis confirms that it is possible to distinguish all stages of pitting corrosion: passive state, metastable state, initiation of pitting, active pitting corrosion state. Characteristic potential oscillations related with pitting corrosion were detected. Research shows that GDEIS method can be with success utilized in the monitoring of pitting corrosion.
Authors
Additional information
- DOI
- Digital Object Identifier link open in new tab 10.1016/j.electacta.2017.09.047
- Category
- Publikacja w czasopiśmie
- Type
- artykuł w czasopiśmie wyróżnionym w JCR
- Language
- angielski
- Publication year
- 2017