Cesium-bismuth-telluride polycrystalline materials were fabricated using a cost-effective method based on a reduction of oxide reagents, leading to a production of a material with good thermoelectric properties. Several samples with various initial stoichiometry were prepared by melting of oxide powders at 1050 °C, quenching, milling to powders and then reducing in pure hydrogen at 400 °C. Another concept was to obtain the CsBi4Te6 material without a melting stage. Composition of the samples was analyzed by the XRD and EDX methods. The sample with 96% of CsBi4Te6 phase was obtained in a way of reduction of oxide reagents. Thermoelectric properties of fabricated samples were also investigated.
Autorzy
- Natalia Gostkowska link otwiera się w nowej karcie ,
- dr inż. Tadeusz Miruszewski link otwiera się w nowej karcie ,
- dr inż. Bartosz Jakub Trawiński link otwiera się w nowej karcie ,
- dr hab. inż. Beata Bochentyn link otwiera się w nowej karcie ,
- prof. dr hab. inż. Bogusław Kusz link otwiera się w nowej karcie
Informacje dodatkowe
- DOI
- Cyfrowy identyfikator dokumentu elektronicznego link otwiera się w nowej karcie 10.1016/j.solidstatesciences.2017.07.016
- Kategoria
- Publikacja w czasopiśmie
- Typ
- artykuł w czasopiśmie wyróżnionym w JCR
- Język
- angielski
- Rok wydania
- 2017