This study examined the changes in the properties of beech wood (Fagus sylvatica L.) after intense drying. Beech wood with false red heartwood was selected as the test specimen. The test samples had dimensions of 50 mm thickness, 180 mm width, and 350 mm length. The specimens were divided into two groups, false red heartwood and sapwood. These specimens were selected with different angles of the growth rings (radial and tangential). The results showed that samples with red heartwood, in comparison to samples with sapwood content, had a remarkable effect in covering. Observation of specimens with false red heartwood and sapwood before and after drying process revealed significant differences in color changes and measured values during the covering-slicing test, but not between samples with different growth ring angles.
Autorzy
- dr hab. inż. Jacek Barański link otwiera się w nowej karcie ,
- dr inż. Aleksandra Konopka link otwiera się w nowej karcie ,
- doc. Ing. Ivan Klement,
- Tatiana Vilkovská
Informacje dodatkowe
- DOI
- Cyfrowy identyfikator dokumentu elektronicznego link otwiera się w nowej karcie 10.15376/biores.12.1.1861-1870
- Kategoria
- Publikacja w czasopiśmie
- Typ
- artykuł w czasopiśmie wyróżnionym w JCR
- Język
- angielski
- Rok wydania
- 2017